Inkoloy
Alloy ea mocheso o phahameng
◆Incoloy800H (Ns112/N08810), Inkoloy800HT, Incoloy800 (Ns111/N08800) ke lihlahisoa tse tharo tsa mofuta o le mong oa nickel-iron-chromium alloy series, li na le ho hanyetsa kutu, ho hanyetsa mocheso le mocheso o phahameng oa oxidation mocheso. kalafo Thepa ea ho kenya, lisebelisoa tse koahelang bakeng sa motsoako oa ho hanyetsa 'mele oa ho futhumatsa li-tubular, lisebelisoa tsa ho lokisa lik'hemik'hale le peterole.
◆Incoloy825 (Ns142/N08825) ke motsoako o akaretsang oa boenjiniere. E na le anti-acid le alkali metal corrosion resistance ka bobeli libakeng tse oxidizing le tse fokotsang. Lintho tse phahameng tsa nickel li etsa hore alloy e be le matla a ho hanyetsa khatello ea maikutlo. E sebelisoa haholo libakeng tse fapaneng tsa indasteri moo mocheso oa ts'ebetso o sa feteng 550 ° C.
◆Incoloy901 ke tšepe e thatafatsang pula, e hananang le mocheso. Alloy e na le matla a lihlahisoa tse phahameng le matla a tšoarellang ka tlase ho 650 ° C, khanyetso e ntle ea oxidation e ka tlase ho 760 ° C, 'me e tsitsitse bakeng sa tšebeliso ea nako e telele. E sebelisoa haholo ha ho etsoa likarolo tse kang likarolo tse fetohang tsa lifofane le lienjine tsa turbine tsa fatše tse sebetsang ka tlase ho 650 ° C.
◆Incoloy925 (N09925) ke tšepe ea alloy e nang le matla a matle a mochine le ho hanyetsa ho hoholo ha kutu. Hangata e sebelisoa ha ho etsoa likarolo tsa ho cheka oli le khase #equipment.
◆Incoloy926 ke tšepe e sa hloekang ea austenitic e nang le lik'hemik'hale tse tšoanang le motsoako oa 904L, naetrojene ea eona e eketseha hoo e ka bang 0.2%, 'me molybdenum e na le 6.5%. E sebelisoa haholo boenjiniere ba marine, tikoloho ea khase ea acid, sistimi ea flue gas desulfurization.
◆Incoloy20 ke mofuta oa thepa ea tšepe e ka sebetsang nako e telele tlas'a mocheso o phahameng ka tlase ho 600 ℃ le khatello e itseng.
◆Incoloy330 e na le matla a phahameng, khanyetso e ntle ea oxidation, ho hanyetsa kutu, ho hanyetsa mokhathala o motle, ho tiea ha fracture le lisebelisoa tse ling, 'me e loketse matla a nyutlelie, indasteri ea lik'hemik'hale le likarolo tse ling tsa mechine.
Sebopeho sa lik'hemik'hale
Kereiti | C | Si | Mn | S | P | Cr | Ni | Fe | Al | Ti | Cu | Mo | tse ding |
ha e kholo ho feta | |||||||||||||
Icoloy800 | 0.1 | 1 | 1.5 | 0.015 | 0.03 | 19-23 | 30-35 | motheo | 0.15–0.6 | 0.15–0.6 | ≤0.75 | - | - |
Inkoloy800H | 0.05–0.1 | 1 | 1.5 | 0.015 | 0.03 | 19-23 | 30-35 | motheo | 0.15–0.6 | 0.15–0.6 | ≤0.75 | - | - |
Inoloy800HT | 0.06–0.1 | 1 | 1.5 | 0.015 | 0.03 | 19-23 | 30-35 | motheo | 0.15–0.6 | 0.15–0.6 | ≤0.75 | - | Al+Ti 0.85–1.2 |
Likoloi825 | 0.05 | 0.5 | 1 | 0.03 | 0.03 | 19.5 ho isa ho 23,5 | 38-46 | motheo | ≤0.2 | 0.6 ho isa ho 1.2 | 1.5-3 | 2.5 ho isa ho 3.5 | - |
Inkoloy901 | 0.1 | 0.6 | 1 | 0.03 | 0.3 | 11-14 | 40-45 | motheo | ≤0.35 | 2.35–3.1 | ≤0.5 | 5 - 7 | Co≤1.0 |
Likoloi925 | 0.03 | 0.5 | 1 | 0.03 | 0.03 | 19.5 ho isa ho 23,5 | 42-46 | motheo | 0.15–0.5 | 1.9 ho isa ho 2.4 | 1.5-3 | 2.5 ho isa ho 3.5 | - |
Likoloi926 | 0.02 | 0.5 | 2 | 0.01 | 0.03 | 19-21 | 24-26 | motheo | - | - | 0.5 ho isa ho 1.5 | 6 - 7 | N15 - 0.25 |
Ikoloy020 | 0.1 | 0.8 | 0.5 | 0.013 | 0.013 | 23.5 ho isa ho 26,5 | - | 13-16 | ≤1.5 | 0.3–0.7 | ≤0.5 | 2.5 ho isa ho 3.7 | - |
Inkoloy330 | 0.04–0.08 | 1 ho isa ho 1.5 | 2 | 0.03 | 0.03 | 18-20 | 34-37 | motheo | - | - | ≤1 | - | - |
Bonyane ba thepa ea alloy
Kereiti | naha | matla a tsitsitseng RmN/m㎡ | Yield Strength Rp0.2N/m㎡ | Elongation As% | Brinell hardness HB |
Icoloy800 | Phekolo ea tharollo | 500 | 210 | 35 | - |
Inkoloy800H | Phekolo ea tharollo | 450 | 180 | 35 | - |
Inoloy800HT | Phekolo ea tharollo | 500 | 210 | 35 | - |
Likoloi825 | Phekolo ea tharollo | 500 | 220 | 30 | - |
Inkoloy901 | Phekolo ea tharollo | 900 | 550 | 25 | - |
Likoloi925 | Phekolo ea tharollo | 650 | 300 | 30 | - |
Likoloi926 | Phekolo ea tharollo | 650 | 295 | 35 | - |
Inkoloy20 | Phekolo ea tharollo | 700 | 300 | 32 | - |
Inkoloy330 | Phekolo ea tharollo | 750 | 310 | 35 | - |