Sebopeho, se bataletseng, se sekwere, se pota-potileng, se setle, se entsoeng ka lesela le se nang letho ASTM A167, AMS 5523
Kopo
Likarolo tsa sebōpi
Lichelete tsa Mocheso
Pampiri Mill Thepa
Likarolo tsa Exhaust ho Li-turbine tsa Khase
Likarolo tsa Enjine ea Jet
Thepa ea ho Hloekisa Oli
Khemistri e Tloaelehileng
Khabone | 0.080 boholo |
Manganese | 2.00 max |
Silicone | 0.75 boholo |
Chromium | 24.00- 26.00 |
Nickel | 19.00-22.00 |
Molybdenum | 0.75 boholo |
Phosphorus | 0.040 boholo |
Lintho Tsa 'Mele
Botenya | 0.29 lbs/in³ 9.01 g/cm³ |
Ho hanyetsa Motlakase | microhm-in (microhm-cm) |
68°F (20°C) | 37.0 (94.0) |
Mocheso o khethehileng | BTU/lb/°F (kJ/kg•K) |
32-212°F (0-100°C) | 0.12 (0.50) |
Thermal Conductivity | BTU/hr/ft²/ft/°F (W/m•K) |
Ho 212°F (100°C) | 8.0 (13.8) |
Ho 932°F (500°C) | 10.8 (18.7) |
Bolela Coefficient ea Katoloso ea Thermal | ka/ka/°F (μm/m•K) |
32-212°F (0-100°C) | 8.0 x 10 (14.4) |
32-600°F (0-315°C) | 9.3 x 10 (16.7) |
32-1000°F (0-538°C) | 9.6 x 10 (17.3) |
32-1200°F (0-649°C) | 9.7x 10 (17.5) |
Modulus ea Elasticity | KSI (MPa) 29.0 x 10³ (200 x 10³) ka tsitsipano 11.2 x 10³ (78 x 10³) ka torsion |
Magnetic Permeability | H = 200 Oersteds |
Annealed | <1.02 max |
Melting Range | °F (°C) 2550 - 2650 (1399 - 1454) |
Thepa ea Mechini
Thepa ea Mechini Ka Mocheso oa Kamore
LETLOTLO | TSIETSO |
Matla a ho qetela a Tensile | 75 KSI mets (515 MPA mets) |
Matla a Kotulo (0.2% offset) | 30 KSI mets (205 MPA mets) |
Elongation | 40% min Ho thatafala Rb 95 max |
Thepa | Tempered 310S e ka fanoa ka maemo a fapaneng a halefileng. |
Ikopanye le Ulbrich Technical Service bakeng sa lintlha tse ling.
Khanyetso ea Corrosion
Sheba ho NACE (National Association of Corrosion Engineers) bakeng sa likhothaletso.
Properties Tempered Alloy 310S e ka phuthoa ho fihlela thepa ea khalefo e hlokoang ke bareki ba itseng le/kapa litlhoko tsa tlhahiso. Ikopanye le Ulbrich Wire bakeng sa lintlha.
Mefuta
Likhoeli tse Tsoelang Pele Khaola ho isa bolelele Precision cutting
Cold Forming Alloy 310S e na le ductility e ntle mme e ka phuthoa, ea etsoa setempe le ho huloa habonolo.
Heat Treatment Alloy 310S e ka thatafatsoa feela ke ho sebetsa ho batang.
Welding Bakeng sa liphetho tse ntle sheba: SSINA's “Welding of Stainless Steels and Other Joining
Mekhoa”.
Meeli ea Boikarabello le Boithorollo ba Tiisetso: Ha ho ketsahalo e tla ba Ulbrich Stainless Steels and Special Metals, Inc., ba tla ikarabella bakeng sa litšenyehelo tse bakoang ke ts'ebeliso ea tlhaiso-leseling e kenyellelitsoeng tokomaneng ena kapa hore e loketse 'likopo' tse boletsoeng. Re lumela hore tlhahisoleseling le lintlha tse fanoeng li nepahetse ho latela tsebo ea rona, empa data eohle e nkuoa e le ea bohlokoa feela. E etselitsoe litšupiso le tlhaiso-leseling e akaretsang mme ha e khothalletsoe bakeng sa litlhaloso, moralo kapa merero ea boenjiniere. Ulbrich ha e fane ka tiisetso e itseng kapa e hlakileng mabapi le popo kapa ho nepahala ha lintlha tse fanoeng tokomaneng ena.