Hastelloy ke motsoako oa Ni-Mo o nang le k'habone e tlase haholo le silicon, e fokotsang pula ea li-carbide le mekhahlelo e meng libakeng tse anngoeng ke mocheso, ka hona e netefatsa ts'ebetso e ntle ea weld esita le sebakeng se cheselitsoeng.Khanyetso ea kutu.Joalo ka ha bohle re tseba, Hastelloy e na le khanyetso e ntle ea kutu mecheng e fapaneng ea ho fokotsa, mme e khona ho mamella ho bola ha hydrochloric acid ka mocheso ofe kapa ofe le khatello leha e le efe tlas'a khatello e tloaelehileng.E na le khanyetso e ntle haholo ea kutu ka har'a acid e mahareng e se nang oxidizing ea sulfuric acid, likhakanyo tse fapaneng tsa asiti ea phosphoric, asiti ea mocheso o phahameng oa acetic, asiti ea formic le li-organic acid tse ling, asiti ea bromic le khase ea hydrogen chloride.Ka nako e ts'oanang, e boetse e hanyetsana le ho bola ka li-catalyst tsa halogen.Ka hona, Hastelloy e atisa ho sebelisoa mefuteng e sa tšoaneng ea peterole le lik'hemik'hale tse thata, tse kang distillation le mahloriso a hydrochloric acid;alkylation ea ethylbenzene le low-pressure carbonylation ea acetic acid le mekhoa e meng ea tlhahiso.Leha ho le joalo, e fumanoe ts'ebelisong ea indasteri ea Hastelloy ka lilemo tse ngata:
(1) Ho na le libaka tse peli tsa sensitization sebakeng sa Hastelloy alloy tse nang le tšusumetso e kholo ea ho hanyetsa ho bola ha intergranular: sebaka se phahameng sa mocheso oa 1200 ~ 1300 ° C le sebaka se bohareng sa mocheso oa 550 ~ 900 ° C;
(2) Ka lebaka la karohano ea dendrite ea tšepe ea weld le sebaka se amehileng ke mocheso oa motsoako oa Hastelloy, mekhahlelo ea intermetallic le carbides e phalla haufi le meeli ea lijo-thollo, e leng se etsang hore e be bonolo haholoanyane ho senya ha intergranular;
(3) Hastelloy e na le botsitso bo fokolang ba mocheso mochesong o mahareng.Ha lihlahisoa tsa tšepe ka har'a Hastelloy alloy li oela ka tlase ho 2%, motsoako o na le maikutlo a ho fetoha ha karolo ea β (ke hore, Ni4Mo phase, motsoako o laetsoeng oa intermetallic).Ha motsoako o lula mocheso oa 650 ~ 750 ℃ nako e teletsana, karolo ea β e thehoa hang-hang.Ho ba teng ha karolo ea β ho fokotsa ho tiea ha Hastelloy alloy, ho etsa hore e be le maikutlo a khatello ea maikutlo, esita le ho baka Hastelloy alloy Kakaretso ea mocheso) le thepa ea Hastelloy e senya tikolohong ea tšebeletso.Hajoale, mekhoa e tloaelehileng ea tlhahlobo ea ho hanyetsa kutu ea intergranular ea li-alloys tsa Hastelloy tse khethiloeng ke naha ea heso le linaha tse ling tsa lefats'e ke mokhoa o tloaelehileng oa ho belisa hydrochloric acid, mme mokhoa oa tlhahlobo ke mokhoa oa ho theola boima ba 'mele.Kaha Hastelloy ke alloy e hanyetsanang le hydrochloric acid corrosion, mokhoa o tloaelehileng oa khatello ea ho belisa hydrochloric acid ha o na kutloelo-bohloko ho leka mokhoa oa intergranular corrosion oa Hastelloy.Litsi tsa lipatlisiso tsa mahlale tsa malapeng li sebelisa mokhoa o phahameng oa mocheso oa hydrochloric acid ho ithuta li-alloys tsa Hastelloy mme li fumane hore ho hanyetsa kutu ha li-alloys tsa Hastelloy ha hoa itšetleha feela ka sebopeho sa eona sa lik'hemik'hale, empa hape le ts'ebetsong ea eona ea ho laola mocheso.Ha mokhoa oa ho sebetsana le mocheso o laoloa ka mokhoa o sa lokelang, eseng feela lithollo tsa kristale tsa li-alloys tsa Hastelloy tse hōlang, empa hape le karolo ea σ e nang le Mo e phahameng e tla fokotseha pakeng tsa lijo-thollo., moeli oa lijo-thollo o kenang botebo ba poleiti e mahoashe le poleiti e tloaelehileng e ka ba habeli.
Nako ea poso: May-15-2023