ALLOY 600 MATERIAL DATA SHEETS
Tekheniki Bulletin
Liforomo tsa Sehlahisoa tse Teng: Pipe, tube, sheet, strip, plate, round bar, flat bar, forging stock, hexagon, terata le extruded section
NEL alloyEL motsoako oa HX
INCONEL motsoako oa 22
Sebopeho sa Lik'hemik'hale % bakeng sa Inconel Alloy 600
Lebitso la UNS | N06600 |
Inconel Alloy | 600 |
Nickel (hammoho le Cobalt) | 72 mets. |
Chromium | 14.0 - 17.0 |
Tšepe | 6.00 - 10.00 |
Khabone | 0.15 max. |
Manganese | 1.0 boholo. |
Sebabole | 0.015 boholo. |
Silicone | 0.50 max. |
Koporo | 0.50 max. |
Tlhokomeliso: Li-alloys tsena li ka hlalosoa ho lihlopha tse thibelang ho fetaka tatellano e itseng.
INCONEL alloy 600 e khethiloe e le
UNS N06600
Nomoro ea Werkstoff 2.4816.
Alloy e amohetsoe tlas'a Boiler le Pressure Vessel Code ea Mokhatlo oa Amerika oa Baenjiniere ba Mechini.E amohetsoe tlas'a Karolo ea I (Li-Boilers tsa Matla), Karolo ea III (Lijana tsa Nyutlelie), le Karolo ea VIII (Lijana tsa Khatello).Likhatello tse lumelletsoeng tsa moralo li fumaneha Karolong ea II, Karolo ea D. Karolo ea I e fanoa ke Code Case 1827.
Molamu, Bar, Wire le Forging Stock
ASTM B 166/ASME SB 166, ASTM B 564/ASME SB 564, ASME Code Cases 1827 le N-253, SAE/AMS 5665 le 5687, BS 3075NA14 le 3076NA14, DIN 17752, 3 ISO 752, 3752 , le 9725, MIL-DTL-23229, QQ-W-390.
Letlapa, Leqephe le Lekhapetla
ASTM B 168/ASME SB 168, ASTM B 906/ASME SB 906, ASME Code Cases 1827 le N-253, SAE/AMS 5540, BS 3072NA14 le 3073NA14, DIN 17750, ISO 62089 ENTL 62089, ENTL 62089, M2089
Pipe le Tube
ASTM B 167/ASME SB 167, ASTM B 163/ASME SB 163, ASTM B516/ASME SB 516, ASTM B 517/ASME SB 517, ASTM B 751/ASME SB 751, ASTM B 775/8529 ASTM /ASME SB 829, ASME.
Linyeoe tsa Khoutu1827, N-20, N-253, le N-576, SAE/AMS 5580, DIN 17751, ISO 6207, MIL-DTL-23227.
Tse ding- ASTM B 366/ASME SB 366, DIN 17742, ISO 4955A, AFNOR NC15Fe