Hastelloy C-276 MATERIAL DATA SHEETS
Tlhaloso ea Sehlahisoa
HT PIPE e fana ka Hastelloy C276 Nickel alloy round bar, Alloy C276 Bar mofani oa thepa Chaena.2.4819 bar e chitja, Alloy C276 rod, UNS N10276 rod, Alloy C276 flat Bar, Hastelloy C276 hollow bar, Hastelloy C276 Nickel alloy round bar supplier, exporter.
Litšobotsi tsa Hastelloy C276 ke life?
● Ho hanyetsa kutu ho hoholo ho fokotsa maemo a tikoloho
● Ho hanyetsa ka mokhoa o ikhethang metsoako e matla ea matsoai a oxidizing, a kang ferric le cupric chlorides.
● Likahare tse phahameng tsa nickel le molybdenum li fana ka khanyetso e ntle ea kutu ho fokotsa tikoloho
● Khabone e tlaase e fokotsang ho na ha carbide e nang le lijo-thollo nakong ea tjheseletsa e le hore e lule e hanyetsana le kutu libakeng tse anngoeng ke mocheso tsa manonyeletso a cheselitsoeng.
● Ho se mamelle ho bola sebakeng se kang pitting le stress-corrosion cracking
● E 'ngoe ea lisebelisoa tse fokolang tse ka mamellang litlamorao tse senyang tsa khase e metsi ea chlorine, hypochlorite le chlorine dioxide.
Hastelloy C276 Nickel alloy round bar Sebopeho sa Lik'hemik'hale,%
Ni | Mo | Cr | Fe | W | Co | Mn | C | V | P | S | Si |
Mesala | 15.0-17.0 | 14.5-16.5 | 4.0-7.0 | 3.0-4.5 | 2.5 max | 1.0 boholo | .01 boholo | .35 boholo | .04 boholo | .03 boholo | .08 max |
Litlhaloso
Litlhaloso tsa ASTM
Pipe Smls | Pipe Welded | Tube Smls | Tube e Welded | Leqephe/Letlapa | Sebaka | Ho qapa | E loketseng | Mohala |
B622 | B619 | B622 | B626 | B575 | B574 | B564 | B366 |
Hastelloy C276 Thepa ea 'mele
Sebaka se qhibilihang: 1325-1370 ℃
Boima: 8.90 g/cm3
Alloy C276 Bar Mechanical Properties
Thepa ea mechine | Tensile, min, ksi[MPa] | Yield, min, ksi[MPa] | Elongation, %(mets) |
Hastelloy C276 | 100[690] | 41[283] | 40 |
Thepa e Tloaelehileng ea Thempereichara ea Kamore ea Lintho Tse Aneloang
Foromo ea Sehlahisoa | Tensile (ksi) | .2% Tlhahiso (ksi) | Elongation % |
Sebaka | 110.0 | 52.6 | 62 |
Letlapa | 107.4 | 50.3 | 67 |
Leqephe | 115.5 | 54.6 | 60 |
Tube & Pipe | 105.4 | 45.4 | 70 |